Apply To CR-10S, CR-10S -S5, CR-10S -S4, CR-10, CR-10 -MINI, CR-20, CR-20 PRO, Ender3 PRO
Compatible with TronXY X5S
Compatible with Tevo Tornado
Compatible with Alfawise U20CR-10S
Marline Configuration:
*13:100k Hisens 3950 1% up to 300°C for hotend "Simple ONE " & "Hotend "All In ONE"
#define TEMP_SENSOR_0 13
https://github.com/MarlinFirmware/Marlin/blob/1.1.x/Marlin/thermistortable_13.h
Recommended slicer setting:
retraction speed over 80MM/S
retraction length 2.5-4MM
If you are facing PLA clogging problem, please try the followings:
1. Increase the retraction speed. The speed may have being limited in the firmware try to change it. G-command "M203 E200"
2. Increase the extruder acceleration. Check your firmware settings. G-command "M201 E9000"
3. Reduce the retraction length. It depends on your machine setup.
4. Increase the nozzle temperature by 5-10 degrees.
5. Do not install the 2 screws for support the heatblcok like the stock hotend on the CR-10 printer.
6. Make sure that there is no gap between the heatsink and the heat breaker.